GrindWeld
OK 75.78 - Image 1
ESAB·consumable

OK 75.78

OK 75.78 is a high‑strength low‑alloy stick electrode designed for steels with tensile strengths over 900 MPa and impact values above 47 J at –60 °C.

Key Features

  • Provides tensile strength > 900 MPa and impact energy > 47 J at –60 °C
  • VacPac™ hermetically sealed, vacuum‑packed packaging for moisture‑free storage
  • Straight‑from‑the‑pack use; no re‑baking required
  • Basic coating on a CrNiMo alloy core

Specifications

  • Classifications: EN ISO 18275‑A : E 89 6 Z B 32 H5
  • Welding Current: AC, DC+
  • Diffusible Hydrogen: 4.0 ml/100 g
  • Alloy Type: CrNiMo
  • Coating Type: Basic
  • Minimum AC Open‑Circuit Voltage: 65 V
  • Tensile Yield Strength: 922 MPa (As Welded, ISO)
  • Tensile Strength: 974 MPa (As Welded, ISO)
  • Elongation: 19 % (As Welded, ISO)
  • Charpy Impact (–60 °C, As Welded, ISO): 47 J
  • Typical Weld Metal Composition: C 0.052 %, Mn 1.91 %, Si 0.30 %, Ni 3.23 %, Cr 0.52 %, Mo 0.63 %
  • Deposition Data (Diameter – Amps – Volts – Efficiency – Fusion Time – Deposition Rate):
    • 2.5 × 350 mm: 70‑110 A, 24 V, 61 %, 52 s, 0.9 kg/h
    • 3.2 × 350 mm: 110‑150 A, 24 V, 63 %, 77 s, 1.4 kg/h
    • 4.0 × 450 mm: 150‑200 A, 24 V, 65 %, 86 s, 1.9 kg/h

Applications

  • Structural steel welding requiring high tensile and impact performance
  • Cold‑temperature service (down to –60 °C)
  • Projects needing reliable, moisture‑free electrodes straight from the pack

Reviews

0 reviews

Write a Review

Be the first to review this product.

Specifications

Alloy TypeCrNiMo
Min Ac Ocv65
Coating TypeBasic
Charpy Impact J47
ClassificationsEN ISO 18275-A : E 89 6 Z B 32 H5
Deposition Data[object Object],[object Object],[object Object]
Welding CurrentAC, DC+
Elongation Percent19
Yield Strength Mpa922
Composition Percent[object Object]
Tensile Strength Mpa974
Charpy Testing Temp C-60
Diffusible Hydrogen Ml Per 100g4.0

Where to Buy